Signs Your Brick Needs Tuckpointing

Tuckpointing is the repair of the mortar joints in a brick or stone wall: the old, failed mortar is ground out and the joints are packed with new mortar matched to the wall. Brick itself can last a very long time. The mortar between it wears out sooner, and when it does, water starts getting into the wall.

In Kansas City that matters more than in a lot of places. The metro gets many freeze-thaw cycles every winter. Water that gets into an open joint freezes, expands, and pushes the masonry apart, so small problems get bigger each year. Here are the signs to look for on your house, chimney, steps, and foundation.

1. Mortar that sits back from the face of the brick

Run your eye along the joints. Sound mortar sits about flush with the brick or in a neat, even tooled line. When the mortar has worn back a quarter inch or more, water collects in the joint instead of running off the wall. Recessed joints are usually the first sign, and the easiest time to repoint.

2. Mortar that is cracked, sandy, or crumbles when you scratch it

Press a key or screwdriver into a joint. Good mortar is hard. If it scratches out like sand or comes out in chunks, it has lost its bond. Hairline cracks running along the joints, or stair-step cracks running up through them, also let water in.

3. Gaps, holes, or missing mortar

Joints with mortar missing altogether are an open path for water, insects, and sometimes small animals. You see this most at the top of chimneys, under window sills, at the base of walls, and around downspouts where the wall stays wet.

4. Spalled or flaking brick

Spalling is when the face of a brick pops off or flakes away. It usually happens after water gets into the brick and freezes. Spalled brick near open joints is a sign water has been getting in for a while. The broken brick needs replacing, and the joints around it need repointing so it doesn’t happen again.

5. White powder or staining on the wall

A white, chalky deposit on brick is efflorescence: salts carried out of the masonry by water as it dries. A little after a wet spell can be normal. Heavy or returning efflorescence, or dark water stains below a joint or chimney crown, means more water is moving through the wall than should be.

6. Damp spots, leaks, or loose brick inside

Water stains on an interior wall or ceiling near a chimney, a damp basement wall, or mortar dust piling up at the base of a foundation wall can all trace back to failed joints. Loose bricks you can wiggle by hand mean the joints have failed badly enough that the bricks may need to be reset, not just repointed.

Where to look first

  • The top of the chimney and the crown, where weather hits hardest.
  • Walls on the side of the house that gets the most wind-driven rain.
  • Under window sills, gutters, and downspouts.
  • The bottom few courses of brick, near the ground, and the foundation.
  • Brick steps, stoops, and retaining walls that stay wet.

Why the right mortar matters

Older brick and limestone are softer than modern brick. The new mortar should be softer than the masonry around it, so that if the wall moves, the joint takes the stress instead of the brick. Mortar that is too hard can crack old brick. Good tuckpointing also matches the color and the joint profile of the existing wall so the repair blends in.

It also helps to repair before sealing. Sealing over failed joints traps water instead of keeping it out. See masonry waterproofing and sealing for how the two fit together.